Oak & Walnut Staircase


This unique spiral staircase was designed and built by Dean Wolfe of
Manchester, California. Dean used WEST SYSTEM® 105 Resin with either 205 Fast or 206 Slow
Hardener, depending on the time need to assemble a part. 403 Microfibers was the adhesive
filler for all bonding operations.

He used red oak for the laminated tread support knees (below) and for
the balusters. The stair treads and handrail are laminated black walnut. The handrail was
laminated as one piece, using the completed stair tread as a clamping jig (below).


The stair treads received two coats of 105/207 Special Coating Hardener
and four coats of semi-gloss polyurethane. The knees, balusters and handrails also
received four coats of polyurethane.

Epoxyworks 15 / Spring 2000
Copyright © 2002, Gougeon Brothers, Inc. All rights reserved.
This page is maintained by Gougeon Brothers, Inc. Last Modified on 10/28/02.
Reproduction in any form, in whole or in part, is expressly forbidden without the consent of the publisher. EPOXYWORKS, Gougeon Brothers, WEST SYSTEM, Episize, Scarffer and Microlight as used throughout this publication, are trademarks of Gougeon Brothers, Inc., Bay City, Michigan, USA.
|