Laminated construction gives lasting
value
John McKibbin recently sent pictures
of his refinished 18' canoe. He built it twenty-five years ago, using cold-molded,
that is, laminated composite construction, with WEST SYSTEM® epoxy. Laminating
a hull is similar to making your own plywood on a three dimensional mold. While
it may take more time and effort to make a laminated hull, the results are well
worth it to many.

John used four layers of 1/20" (0.050")
veneer for the canoe. The outer skins are made from American walnut and the
interior layers are Port Orford cedar. He chose the cedar as the interior "core"
because of its light weight and strength. He chose the walnut because of its
beauty, rot resistance, and high strength-to-weight ratio. Laminating the walnut
with epoxy greatly increased the compression strength of the wood and helped
the entire structure's stiffness. The hull was stiff enough at the gunnels that
John felt it didn't need thwarts, commonly used on canoes this size. The inwales,
seat supports and decks were cleverly designed into the form and were molded
right in the hull. The hull has a total weight of 55 pounds, not bad for an
18' canoe.
Twenty-five years provides a true
test of time and durability for WEST SYSTEM epoxy, especially with a species
of wood not commonly used in boat building. John's canoe testifies elegantly
to the beauty and lasting value that laminating with epoxy can bring.
Epoxyworks 18 / Fall 2001
Copyright © 2002, Gougeon Brothers, Inc. All rights reserved.
This page is maintained by Gougeon Brothers, Inc. Last Modified on 10/28/02.
Reproduction in any form, in whole or in part, is expressly forbidden without the consent of the publisher. EPOXYWORKS, Gougeon Brothers, WEST SYSTEM, Episize, Scarffer and Microlight as used throughout this publication, are trademarks of Gougeon Brothers, Inc., Bay City, Michigan, USA.
|