by Bruce Niederer — GBI Technical Advisor

Above: Our study of adding pigments to epoxy.

We often get asked ‘What can I use to color my epoxy?’ The intended application is as varied as our customers. Often it’s simply to make it easier to paint over or to provide a color indicator between layers. Sometimes it’s to match a particular colored material in a repair. Maybe it’s for an art or craft project. The point is, people are often looking for a color other than the black 423 Graphite, 501 White or 503 Gray Pigments offered in the WEST SYSTEM® product line. What are some options for adding pigments to epoxy? And what are the pigment’s effects on the performance of the epoxy? (more…)