By Jeff Wright — Vice President of Technical Services
WEST SYSTEM® Six10 is a two-part, pre-thickened epoxy adhesive formulated with properties that make it perfect for many adhesive applications. Compared to other ready-to-dispense adhesives, its particular physical properties make it ideal for stitch and glue boat construction, fiberglass laminate repair and general bonding. This new formulation has a good balance between the elongation and toughness of G/flex® and the strength and stiffness of our 105 Resin-based epoxies. You can use it with as many materials as possible including wood, metals and composites. The long working time with fast thru-cure and unique shear thinning are additional characteristics formulated into Six10 that contribute to its ease of use. (more…)