Monthly Archives: September 2015

First Place winner at MITES

Pedal Car

By Jon Fox

Epoxyworks 41

Cover Photo: First place winner at MITES at both the regional and state level.

For the past two years, the Drafting/Pre-Engineering class I teach at Tuscola Technology Center in Caro, Michigan has been invited to participate in a contest sponsored by Summit Racing.  Students build a custom pedal car that is displayed and judged at the AutoRAMA show at Cobo Hall in Detroit. Summit Racing either supplies participating schools with one of their stock pedal cars which can be modified and customized, or students may build their entry from scratch. We constructed our entry from scratch both years. Our first car was inspired by the Delehaye roadster and built of aluminum in an Art Deco style. Continue reading

National Sailing Hall of Fame

By Grace Ombry

Meade and Jan Gougeon were inducted into The National Sailing Hall of Fame (NSHOF) in October of 2015. Meade and Jan, along with their brother Joel, founded Gougeon Brothers, Inc. in 1969. They were selected because of their pioneering work in the use of epoxies for boat construction, and because each are accomplished sailors. Continue reading

fiberglassing overhead

Techniques for Fiberglassing Overhead

By Tom Pawlak — GBI Technical Advisor

The prospect of fiberglassing overhead when laminating the bottom of a hull can be a bit ominous. Any type of overhead work can be frustrating, but the thought of trying to hold fiberglass in place while applying epoxy can produce nightmares for some people. This is especially true if you will be working alone. Continue reading

carbon fiber air scoop

Carbon Skinning

Why reinforce with carbon fiber?

By Don Gutzmer

Carbon fiber has very high strength-to-weight ratios and higher stiffness compared to many other reinforcing fabrics. These special properties make it ideal for applications in aerospace, automotive, military, and even sporting goods. When combined with a WEST SYSTEM Epoxy it can be used to build high-end composite parts. Continue reading

Blake jumps with his motocross bike

The Carbon Fiber Look

By Daryl Burnett

I was talking to my friend Blake Rivard about doing something different for his motocross bike. We settled on a carbon fiber airbox (air filter cover). On his bike, the airbox sits just below the handlebars where the gas tank usually is. I started with removing the plastic piece and cleaned it so no dirt would be present in the final product.  The original airbox would serve as a mold for the finished piece. Continue reading

Big Jon Needs a Little Help

By Tom Pawlak — GBI Technical Advisor

Big Jon (BJ) serves as a reel for retrieving and letting line attached to floating planer boards in and out from a boat while trolling. Planer boards are used to get fishing lures off to the side of the hull so the lures aren’t following directly behind the boat while trolling for walleye. The further the planer board is reeled out, the further the lures are from the side of the hull. BJ has served Tom and Lorraine Klinski well but recently developed some cracks in what appears to be a black nylon plastic. Continue reading

testing boats in the creek

Hartland Boatbuilding

By Matt Assenmacher

As summer approaches, keeping students interested in learning while wrapping up the school year can be a challenging task. I teach mechanical engineering at Hartland high school in Hartland, Michigan. My students learn the principals of technical design while guiding through a fun, hands-on, year-end design project. Continue reading

West System Epoxy

That’s a Fact!

Useful information about WEST SYSTEM Epoxy

By Mike Barnard

Using gelcoat over WEST SYSTEM

It’s a myth that if you plan to gel coat over a repair, you must make the repair with polyester. We’ve used gel coat over epoxy for decades, shown it in our instructional videos on repairing fiberglass boats, and discussed it in past issues of Epoxyworks. Continue reading