Author Archives: ewadmin

Readers’ Projects, Issue 12

Battleship Replica

This battleship replica was built by Rob Neill of Naples, Florida. He began building models after retiring from his job at the local power company. He spent two years building the 15′ radio-controlled replica of the Iowa class Battleship, New Jersey, using wood, WEST SYSTEM epoxy and brass. Starting from scratch, he completed a set of plans by scaling photographs and drawings from library books, then lofted a mold from the plans. Continue reading

Set Building with WEST SYSTEM® Epoxy

By Ron Sherry

The Society of Automotive Engineers (SAE) asked Composite Concepts, Inc. to build a three dimensional version of the SAE logo for the SAE International Congress Banquet in Detroit, Michigan. An easy feat, until you consider the size of the letters. They are 22′ tall, 56′ wide and 4′ deep, with a horizontal 2′ high split down the middle. Add some projection and neon lighting, and you have an impressive back drop for the engineers receiving their awards at this black tie dinner. The speakers entered the stage from under the letter A before they approached the lectern. Continue reading

Repairing a Runabout Floor or Pontoon Deck

By Joe Parker

A common source of problems on open runabouts and pontoon boats is the cockpit floor or deck. This part of the boat is usually just a layer of plywood screwed down to the top of stringers and frames. Many have a layer of carpet or vinyl flooring material glued onto the plywood. Continue reading

Stringer Repairs in Fiberglass Boats

by Brian Knight

Epoxyworks 11

Cover Photo: Fiberglass boats can be repaired with WEST SYSTEM Epoxy.

Fixing damaged or delaminated stringers is one of the most common repairs associated with fiberglass boats. The usual causes of stringer failure are disintegration of the stringer core material, impact damage from slamming and grounding, and fatigue from normal use. Although each repair situation has its own unique problems, the following techniques are fundamental to stringer repair. These guidelines will help you repair almost any damaged stringer. Remember, stringers are structural support members. As you repair or replace damaged material, use your best workmanship. Continue reading

Jubilee Sailing Trust (Tenacious) Project

Courtesy of Wessex Resins & Adhesives, Romsey, England

At the Jubilee Yard in Southampton England, progress continues on the Jubilee Sailing Trust ship. The ring frames are all erected, and for a short period, the completed skeleton of the ship resembled a giant toast rack. Continue reading

Techniques for Fiberglassing Overhead

By Tom Pawlak — GBI Technical Advisor

The prospect of having to fiberglass the bottom of a hull can be a bit ominous. Any type of overhead work can be frustrating, but the thought of trying to hold fiberglass in place while applying epoxy can produce nightmares for some people. This is especially true if you will be working alone. Continue reading

Repairing Fiberglass Powerboat Transoms

By Tom Pawlak — GBI Technical Advisor

Transoms are major structural parts of fiberglass powerboats, especially outboards. Transoms not only support the weight of the motor, they maintain the shape of the boat, they are a mounting point for holdowns, towing eyes and other accessories. And, they must be able to let water out of the hull, without letting it back in. Continue reading

Table Top Applications

By Captain James R. Watson

Pouring a thick coating of epoxy onto a table top can produce a unique effect. With a ¼” thick coating you can cast a variety of objects in the epoxy for decorative accents. Coins, fabrics, sticks of wood, memorabilia and photographs have been used in this decoupage application. Here are a few tricks to make things go more smoothly. Continue reading