planter box 2 ← Previous Next → 2—The ¼” gap at the edge of the plywood sides was filled with thickened epoxy. A layer of glass tape was laid over the corner and smoothed into the thickened epoxy. The glass was then wet out with epoxy and the edges were sanded smooth when cured.