A properly engineered Scootboard chassis. Even without the resources of a well-equipped test lab, Bill Bertelsen, GBI’s test engineer, was able to gather useful composites data using the equipment at hand—in this case, a spring clamp, a ruler, a digital camera, and an 8-year-old girl.