Tag Archives: 34

Building a Custom Stained Glass Mold with G/5

By Tom Pawlak — GBI Technical Advisor

A few years back Mary, my better half, suggested I make a stained glass lamp for our den at home. There are molds commercially available for making glass lampshades. They hold glass pieces in position in the desired curved shape until the soldering process is complete. Unfortunately, the shape I wanted was not available. I wanted something similar in size and shape to the fabric-covered lamp shade in the den. In the end, I decided to make a custom mold. Continue reading

Skeg Construction for SPARKS

By Ted Moores

This article is Lesson 3 of a series. See bottom of page for links to additional articles in this series.—Ed.

Designing and building a successful skeg for Sparks (our 30′ hybrid electric launch featured in Epoxyworks 32) took some head scratching. But in the end, it was just another combination of wood and WEST SYSTEM® epoxy. Our skeg needed to be functional and age gracefully, yet be reasonably quick and easy to build and install. This project was an ideal opportunity to explore the limits as well as the advantages of combining wood with epoxy to engineer simple solutions to complex problems. Continue reading

The Coupe de Ville of Epoxy Caddies

By Mike Barnard

My father has grown very fond of WEST SYSTEM® Epoxy and his box of epoxy-related items has been growing at a steady rate. The overflow of his box in an already “treasure” packed garage emphasized his need for an organization and storage system for these materials. We have had several requests for this same type of solution lately, so I did some digging and found a great Boatbuilder article from 1986 written by J.R. Watson. Inspired by this article, my father and I built our own interpretation of the Epoxy Caddy.

Transporting epoxy with the 300 Mini-Pumps in the containers is typically awkward with a risk of overturning. The pumps could become damaged, and the alternative, to remove them, is messy and unnecessary. We always store the epoxy with the pumps in place. Inadvertently, a drip will cause a mess. A pot placed under the mini pumps will catch those rascals, but if the containers or the pot are not positioned correctly all’s for naught. The glue caddy solves both transportation and storage problems.

A caddy can be simple or as elaborate as you want. One could design it to become an epoxy work station complete with storage for brushes, stir sticks, hand cleaner, gloves, paper towels and so on. Or it could be designed simply with cutouts for containers and drip pots. One can simplify or expand upon the concept, tailoring to meet your needs.

Set whatever size containers you are going to use together, trace around their bases onto the plywood, and cut it out with a sabre saw. Position the drip pot cutout so it will be under the spouts of the mini pumps. With pots in position, you’re ready to go to work.

1. Lay out the items you want in your caddy on a sheet of plywood. Trace the outline of each item. Be sure to include a drip cup below the resin and hardener mini pump spouts.

2. Cut out the shapes of each item slightly oversized as necessary.

3. Add sides, a bottom and a handle to complete the caddy.

Bubble-Free Coating

By Mike Barnard & Don Gutzmer

WEST SYSTEM® epoxy has long been a popular choice for clear coating table tops. It works great as a buildup coat and a moisture barrier. It also showcases the beauty of wood grain and fiber weaves. Formulated with boat building in mind, WEST SYSTEM epoxy is not intended as a final finish coating. You may find it a bit more difficult to achieve a perfect surface with epoxy than with a coating formulated specifically for final finishing, such as varnish.

However, WEST SYSTEM offers some distinct advantages. It builds up quickly: a single coat of 105 Epoxy Resin® with 207 Special Clear Hardener® offers about four times the thickness of a typical coat of polyurethane varnish. WEST SYSTEM epoxy is also an excellent moisture barrier, stabilizing the surface so your final finish coat will look beautiful longer. Continue reading

Adhesive Bonded Structures

By Jeff Wright — Vice President of Technical Services

Fiberglass reinforced plastic and other composites influence the design of many products manufactured today. Boat hulls, sports equipment and airplanes can easily take new, complex shapes when composites are used in place of traditional materials. Reinforcing structures also benefit from the versatility of composite materials when prefabricated components are bonded with a high-strength adhesive. This article will discuss some of the engineering aspects to consider when designing or repairing an adhesively bonded composite structure. Continue reading

Foam Strip Planking

Foam Strip Plank Boatbuilding

BY JOHN LINDAHL 

A couple of years ago my son Ian asked me about building an A Class catamaran. Having built several of these in the past and knowing what was now on the market, I came up with a build method that would:

  • Allow us to build a competitive design.
  • Be at or under the class minimum weight of 165 lb.
  • Be as strong and stiff as anything on the market.
  • Be competitive in quality and price, but not get trapped in exotic equipment expense. This meant no vacuum bag, no pre-preg, no resin infusion, and no autoclave.

Continue reading

White Oak Redux

White Oak Redux

By Bruce Niederer and Bill Bertelsen

Building stuff, especially boats, with wood is much like a religious calling; once you hear the call, there’s no turning back. Those who’ve heard the call will not suffer fools willingly, so when I decided to conduct some white oak adhesion and shear testing and report the results in Epoxyworks 31, skeptics and believers alike took to the internet wooden boat forums-and had no problem speaking their minds! Having healed from the pummeling I took in some quarters, I’m back again to report the promised follow-up test results. Continue reading

Construction of a Lantern Post

By Donald Stevens

Having thought about constructing a nice lantern post for many years, I was inspired when I read an article in Woodenboat Magazine about building hollow spars with “bird’s mouth” joints. Having a pile of red cedar drops from other projects I came up with the design of using two staved sections connected by a turned collar of the same material.

Continue reading

New Repair Kits

New for 2012, WEST SYSTEM is offering three specialized boat repair kits designed with the do-it-yourselfer in mind. Each contains the right materials and instructions for making lasting repairs and retails for around $30 at your local stocking WEST SYSTEM dealer. Continue reading

Outdoor Sculpture Sculptor

A Little Less Than Meets The Eye is a 9′ x 7′ x 6′, Fiberglass and polished aluminum sculpture installed at Raleigh, North Carolina, Art on City Plaza. 

By Mike Barker

Bill Wood has been making sculptures since high school. He has a degree in Art from Ottawa University, Ottawa, Kansas and attended the Kansas City Art Institute, Kansas City, Missouri. His work has been featured in shows from Connecticut to Key West and as far west as Topeka Kansas. Continue reading