Comparing Surface Preparation Techniques for Paints and Primers

By Joe Parker

Before you begin a project, it is a good idea to consider all of your options. Information about products or methods you may want to use is often available on product labels, from manufacturers, or your own experience. However, many times the information you need to make good choices is just not available. Then your best option is to test. In our most recent renovation, we had to figure out what to test for and how to do it. Continue reading

Bonding to Corian™ and Wilsonart™ Laminates

By Tom Pawlak — GBI Technical Advisor

We recently did adhesion testing to Corian and Wilsonart surfaces with WEST SYSTEM 105 Resin and 206 Hardener at the request of a composite panel manufacturer. Corian and Wilsonart are mineral filled acrylic panels that look like granite and are often used as countertop material in kitchens and offices. Cabinetmakers and contractors typically use the panels in ½” thickness for residential applications. They are quite heavy, though not nearly as heavy as actual granite. Continue reading

Gluing Plastic Dimensional Lumber

By Patrick Ropp

More people are using recycled plastic/wood composite lumber for decks and other various projects. Although each manufacturer of recycled plastic lumber has his own blend, we found that most are using very similar ingredients: an equal amount of melted recycled plastic mixed with recycled wood chips or sawdust and then extruded in the form of dimensional lumber. Since the wood is encased in plastic, the plastic/wood composite boards are supposed to last longer than traditional decking materials and carry a good warranty. Many of these boards are not intended for use as structural members, but they Continue reading

Varnish over epoxy

Testing House Paint Primers

By Tom Pawlak — GBI Technical Advisor

Gougeon Brothers, Inc. regularly engages in testing to support those who use our epoxy in architectural applications, both in new construction and repairs. In the past, we have tested the compatibility of house paint primers over WEST SYSTEM® epoxy and found that a variety of primers worked well. Latex primers especially performed well when applied over cured epoxy, even when the epoxy was marginally prepared prior to painting (Epoxyworks 7, Spring 1996). Continue reading

Thinning WEST SYSTEM Epoxy

By Brian Knight

A question frequently posed to our technical staff is “can I thin WEST SYSTEM® epoxy so it will flow or penetrate better?” The answer to that question is “yes, but not without consequences.” Many of the advantages of thinning epoxy are offset by disadvantages in other areas of epoxy performance.

Continue reading

Low-Tech Adhesion Testing

By Jim Derck

Before beginning a project, it’s a good idea to test the adhesion between epoxy and the materials to be used. Preliminary adhesion tests can help you choose the best materials and surface preparation methods. It can also help to avoid a surprise bonding failure.
At Gougeon Brothers, Inc. we use a Pneumatic Adhesion Tensile Testing Instrument (PATTI) for adhesion tests. After the PATTI test stud is bonded to the test surface, the stud is pulled in tension until it releases. The instrument gauge gives a precise pounds per square inch reading at failure. Continue reading