Climbing Drum Peel Test for Adhesives

By Bruce Niederer

No matter how you use WEST SYSTEM epoxies, you expect us to back up the products and methods we recommend with solid data based on tests that simulate “real life” applications. To this end we began conducting the ASTM 1781-93 test method known as the Climbing Drum Peel for Adhesives. As expected, the results from this test method compliment the data we’ve already compiled using the PATTI (Pneumatic Adhesion Tensile Testing Instrument) meter. Continue reading