Tag Archives: Allied Seabreeze 35

New Window Frames for STARDUST

Casting aluminum- filled epoxy frames

By Joe Parker

To prep our 30-year-old Allied Seabreeze 35 for a paint job, we had to remove the window frames. These frames were cast aluminum and original equipment. The outer frames were thicker and had not been broken. However, once we began to remove the inner frames, it was obvious that they had been removed for previous paint jobs. The aluminum castings had been broken and repaired by simply gluing them back together with an unidentifiable filled adhesive. Continue reading