This is a formula for homemade resin-removing hand soap that we have used around our shops for the last few years. You can make it in the kitchen blender from common household supplies. The beauty of this stuff is that it’s easy on you, easy to make and easy to clean up. This is a recipe sure to please the whole family. Percentages are provided so you can easily customize batch sizes for a small job or a big work crew. Continue reading