Blake jumps with his motocross bike

The Carbon Fiber Look

By Daryl Burnett

I was talking to my friend Blake Rivard about doing something different for his motocross bike. We settled on a carbon fiber airbox (air filter cover). On his bike, the airbox sits just below the handlebars where the gas tank usually is. I started with removing the plastic piece and cleaned it so no dirt would be present in the final product.  The original airbox would serve as a mold for the finished piece. Continue reading