Strings’ Float

By Greg Bull — GBI Technical Advisor

When Jan Gougeon built Strings in 2010 one of the most interesting features he included, at least from my point of view, was the float that goes on top of the mast. Due to its zeppelin-like shape, this is also called a blimp or a dirigible. The purpose of the float is to make the boat self-rescuing: if the boat tips, the float prevents it from going any farther than lying on its side. The mast and float are then used to right the boat. Jan developed this system when designing the Gougeon-32 back in the late ’80s, so he thought it would work for Strings. Continue reading