Tag Archives: Epoxyworks #30

Bicycle Frame Repair vs Wall Art

By Randy Zajac

I will start by saying that, in my opinion, most carbon fiber bicycle frames that have sustained damage from an impact should not be repaired—there are too many damaged fibers that are typically unseen. The two repaired frames featured in this article had damage caused by operator error, not impact. The last two frames are prime examples of parts that should not be repaired for safety reasons. Continue reading

The Artistador

Claudia Toutain-Dorbec is a multi-media artist living in northern New Mexico. The Downey Gallery in Santa Fe asked Claudia to create a life-size sculpture in preparation for the city’s 400th birthday celebration which began Labor Day weekend 2009, and runs for a year. She created the Artistador, a conquistador who is also an artist, seeking his treasure in art.

Continue reading

laminated denim knife handle

Readers’ Projects, Issue 30

Laminated Denim Knife Handle Material

Knife makers Cliff Fendley and Mike Carter decided to try their hand at making laminated denim knife handle material. After some research, they chose to use WEST SYSTEM 105 Epoxy Resin with 206 Slow Hardener to laminate pieces of denim fabric into blocks from which they could machine knife handles. Mike first made a 5″ x 7″ piece about 1/2″ thick with alternating front and back layers of blue jean denim. Cliff made a 1″ thick 5″ x 5″ Piece from faded blue jean and 1″ thick 5″ x 5″ piece from faded blue jean and a 1″ thick 1″ x 7″ piece from alternating layers of tan and black denim which he twisted before pressing.

Continue reading