Tag Archives: Epoxyworks #40

Six10 Adhesive Finds a Home in “Boutique Style” Construction

By Emily Soyka

Epoxyworks 40

Cover photo: Installing some of the assembled FRP louvered panels on the rooftop residence.

Renew Urban Charleston, LLC in Charleston, South Carolina has been using WEST SYSTEM® Six-10 Epoxy Adhesive to glue hundreds of pultruded fiberglass channels and square tubes together to form decorative louvers. When installed on the building, the louver assemblies create an aesthetic detail that draws attention to the unique rooftop residence on King Street in Charleston. Continue reading

502 Black Pigment

502 Black Pigment

by Mike Barnard

On January 1, 2015, we began selling a new WEST SYSTEM Epoxy pigment. We already had the 501 White Pigment and the 503 Gray Pigment, so it seemed right to introduce our new 502 Black Pigment. Just like the 501 and the 503, it alters the color of the epoxy mixture without affecting the cured physical properties. Similarly, the maximum acceptable loading is 3%. This is great for hiding a surface with a single coat of black epoxy. Adding more pigment will increase the opacity, but can skew the mix ratio because there is epoxy resin in the pigment. Continue reading

The Great Lakes Boat Building School Graduates the Class of 2014

By Bruce Niederer — GBI Technical Advisor

I traveled to the U.P. (that’s what we Michiganders call the Upper Peninsula) on June 7th to attend the graduation ceremony and participate in the yearly on site PAC (Project Advisory Committee) meeting which I currently sit on. I arrived on a beautiful sunny day with temperatures in the mid 70s, a stark contrast from my last trip to the school in mid-April when I awoke to 4” of new snow and 3°F! For those of you who live in the southwest where the temperature has been hot for some time, by contrast, the great lakes finally became 100% ice free the beginning of June. Continue reading

Talkin’ the Talk

By Julie Jezowski

Here at GBI, we’re not just your average epoxy “retailer.” We are the leading provider of quality epoxy products and services. Quality epoxy as in; we dream a big, sticky, epoxy dream, research it, develop it and produce it.  Service as in; packed within our 20,000(ish) square foot walls is a wealth of knowledge and experience so vast that it has enabled us to educate hundreds of people worldwide on the features and benefits of West System® epoxy.  Spanning from A to Z….Alaska to Zimbabwe. . Yeah, I know. Alaska. Mind. Blown. Continue reading

Profile of an American Craftsman

By Bruce Niederer — GBI Technical Advisor

I hear it said increasingly often in the last couple years as I meet people during my travels “Who will be the next generation of tradesmen? Who is going to work on our cars, boats and homes?” This is a serious lament posed by today’s tradesmen, potential employers who have a very hard time finding apprentices and workers to learn their trade. The U.S. is in dire need of men and women willing to work with their hands and develop the skills necessary to build and repair all our…stuff. Continue reading

A Rendezvous with History: Les Staudacher & Tempo Alcoa

By Bruce Niederer — GBI Technical Advisor

In my article Profile of an American Craftsman the photos of the Les Staudacher jet-powered boat provide a photographic history of the first and last run of the Tempo Alcoa. What follows are the details of that historic event.

In 1957 Guy Lombardo and the Royal Canadians were in high demand. The band leader and his music were well known throughout the U.S. and Canada. Lombardo was also a successful and well-known driver of Gold Cup hydroplane speedboats. Prior to WWII, Lombardo had a distinguished 225 cubic inch class career and moved up to the Gold Cup circuit after the war when he bought the proven Champion My Sin from Zalmon Simmons in 1948. Continue reading

G/Flex Weds Wood and Glass Crystal Goblets

By Tom Pawlak — GBI Technical Advisor

David Black is a creative boat builder, woodworker and artisan living in San Diego California. He is very familiar with all the WEST SYSTEM Epoxy resin/hardener combinations but recently has become a huge fan of G/flex Epoxy.

I love it when David calls because his projects are always interesting. He pushes the envelope of how epoxy can be used. His clients appreciate him too for his creative abilities. Do you have an idea for a new table for your mega yacht? Call David. Need a unique teak deck for your yacht that no one else will even consider installing? Call David. Need someone to design and build a one-of-a-kind interior for your new motor coach? David is your guy. If it is out of the ordinary and it tests the realm of possibility and good reason, count him in. Continue reading

Dirt Bike Loading Ramp

By Daryl Brunette

A dirt bike loading ramp is very bulky and heavy, but important for loading everything you need in motocross. You can just use a wooden board thick enough to support the weight of your bike, or you can buy expensive aluminum ramps. But I (Daryl) wanted to build one and give it a personal touch, making it lighter and stronger. Continue reading

Fairing Basics

By Jeff Wright — Vice President of Technical Services

The goal of fairing is to create a surface without bumps or hollows.

Fairing Compound should be of a consistency that can be troweled onto a surface without sagging. Add 407 Low Density or 410 Microlight filler to mixed epoxy, checking the consistency as you stir in the filler to determine if the mixture has the correct viscosity for your application.

Continue reading

FIBERwave PAVILION

By Alphonso Peluso and his Spring 2014 IIT Architecture Students Joseph Bertucci, Cecilia Campos, Dijon Dunmore, Xinyun Huang, Jared James, Ryan Kim, Dakotah Lucas, Jeffrey McQuiston, Nick Rienstra, Teresita Pineda, John Seaman & Jeffrey Wigen

The FIBERwave PAVILION was designed and built as part of a student-based design research studio. Carbon fiber was used because when coated with epoxy it can become as hard as steel, and added layers enhance its strength. It offers designers great control over structural properties and is incredibly lightweight. Continue reading