By Jeff Wright — Vice President of Technical Services

The goal of fairing is to create a surface without bumps or hollows.

Fairing Compound should be of a consistency that can be troweled onto a surface without sagging. Add 407 Low Density or 410 Microlight filler to mixed epoxy, checking the consistency as you stir in the filler to determine if the mixture has the correct viscosity for your application.