By Bill Bertelsen
Our Technical Advisor Jim Derck (now retired), noticed that some fabrics seemed to have a remarkable thirst for epoxy. To determine exactly how much epoxy it takes to wet out and bond different kinds of fabric, Jim conducted a carefully controlled experiment. Continue reading