My porch railing at home was badly in need of painting even though I had painted it the summer before. After just one Michigan winter, the paint had cracked and lifted. I wondered to myself if coating the top rail with WEST SYSTEMĀ® epoxy would improve this poor situation and decided to turn the top rail into a small R & D project. Continue reading