Tag Archives: fender

Light as a Feather

How I made a composite fender for my bike

By Tom Pawlak — GBI Technical Advisor

Last Father’s Day I received a new light and sleek bicycle from my family. It is by far the nicest bike I’ve ever owned. I enjoy riding it to work in the spring, summer, and fall. Because it is so nice, I decided I didn’t want to bolt on the aluminum bracket used previously over the back wheel on my old bike. The bracket had served multiple purposes. It supported my travel bag and it acted as a fender to keep road water off my back while riding. I decided I would ride with a backpack instead to reduce bulkiness and thought it would be nice to make a lightweight composite fender that I could snap on for those rainy days. That would allow me to remove it for longer trips and on nice weather days. Continue reading