The Fairing File

My son Matt and I recently built a small stitch-and-glue boat. While fairing the bottom we discovered that hacksaw blades can be modified and used for fairing.

The buildup of fiberglass tape along the chine and keel had caused a low spot in the hull all along the edge of the fiberglass buildup. Filling the low spot with low-density filler was easy, but sanding the cured epoxy with sanding boards was slow work. Experimenting with a new hacksaw blade, we found it easily cut through the low-density filler and occasional high spots in the fiberglass. Continue reading