Tag Archives: flower pot

Pot repair with epoxy

One-Shot Pot Repair

By Tom Pawlak — GBI Technical Advisor

My wife Mary and I recently went to the local building center to purchase a large planter pot for our patio. After we had agreed on a nice large terra-cotta beauty, I noticed another large pot that had a serious crack. I asked the associate for a price on it, knowing it would be easy to repair with WEST SYSTEM® epoxy. He said I would be doing him a favor if I took it away. So we came home with two pots for the price of one. Continue reading