Johnathan Clowes’s Mobiles

Since 1983 the Walpole, New Hampshire sculptor Jonathan Clowes (Clowes Sculpture) has been creating mobiles that hang in institutions and residences across the country. He uses WEST SYSTEM® epoxy as an adhesive and a coating for the wood laminate that form these pieces. Clowes describes his technique:

“In general, the long sinuous parts are formed from stacks of veneers that are bent over a mold to make a rough blank from which the pieces are carved. The most consistently good method for making molds is to bend strap steel or aluminum to the desired shape and support it with sufficient wood scrap bracing to form a backbone. Usually the bracing is held with screws or fillets of epoxy paste. Continue reading