Laminated Denim Knife Handle Material

Knife makers Cliff Fendley and Mike Carter decided to try their hand at making laminated denim knife handle material. After some research, they chose to use WEST SYSTEM 105 Epoxy Resin with 206 Slow Hardener to laminate pieces of denim fabric into blocks from which they could machine knife handles. Mike first made a 5″ x 7″ piece about 1/2″ thick with alternating front and back layers of blue jean denim. Cliff made a 1″ thick 5″ x 5″ Piece from faded blue jean and 1″ thick 5″ x 5″ piece from faded blue jean and a 1″ thick 1″ x 7″ piece from alternating layers of tan and black denim which he twisted before pressing.