Tag Archives: Measuring Epoxy

Positive displacement epoxy pumps

Tools for Measuring Epoxy Quantities

303 and 305 High-Capacity Positive Displacement Pumps

 
305 Metering Pump

 

 

 

Updated Spring 2016

For measuring epoxy accurately, Gougeon Brothers, Inc. has introduced high-volume epoxy pumps that are extremely robust. These pumps dispense epoxy faster than any pump the company has previously offered.  The 303 and 305 Positive Displacement Pumps work by trapping a fixed amount of resin and hardener, then forcing (displacing) that trapped volume into the discharge pipe or system.  The mechanics of this setup mean that increases in resin viscosity due to temperature changes will not slow dispensing speeds. Positive latching lids help prevent contamination of resins and hardeners.

The new 303 Positive Displacement Pump is calibrated for WEST SYSTEM 3:1 ratio epoxies (105 Resin with 207 Special Clear Hardener or 209 Extra Slow Hardener) and is easily identified with a red base. The new 305 Positive Displacement Pump is calibrated for 5:1 ratio epoxies (105 Resin with 205 Fast Hardener or 206 Slow Hardener) and has a blue base.

Positive Displacement Pumps are also available with drum fittings.  These connect directly to WEST SYSTEM Resin and Hardener drums so there is no need to decant materials.  This setup conveniently streamlines the metering process for high-volume users, saving both time and money.

Positive displacement epoxy pumps

Big Batch Mixing Methods

By Tom Pawlak — GBI Technical Advisor

Most of us use epoxy in small batches, mixing several ounces at once. This gets the job done 95% of the time. But for some projects, such as large laminating jobs, you may need large batches of epoxy. Before you begin, you should understand what’s involved in mixing big batches of epoxy. Continue reading