Methodist Church window repair

Revisiting a Church Window Restoration

By J.R. Watson

Those working on projects that use epoxy for restoration and rot repair often ask, “How long will this last? Will the rot return?” At Gougeon Brothers, Inc., we have lots of in-house test approaches that can analyze tension, compression, shear, and fatigue. We can also predict the consequences of ultra-violet, arid, tropical, and cold conditions. Still, there’s nothing like real-world performance over time. Continue reading