Tag Archives: Optimist pram

Estimating Epoxy Amounts

Estimating Epoxy Amounts

By Bruce Niederer — GBI Technical Advisor

This formula will help you estimate the amount of mixed epoxy needed to wet out fiberglass cloth (assuming a resin-to-fiber ratio of 50:50) and apply three rolled epoxy coats to fill the weave of the cloth, i.e. “fill coats.”

The formula includes a waste factor of approximately 15%; however, more (or less) may be needed depending on the job and personal application technique. The epoxy is applied at standard room temperature, approximately 72° F. Continue reading