I wanted to purchase a personal watercraft so I’d be able to join my friends at the local lake for some fun in the sin this summer.  Like most people on a budget, I searched Craigslist for the best deal.  I needed something low maintenance, so a WaveRunner™ felt like a good fit.  After a week of looking, I found a 2004 Yamaha GP1300r that appeared to be in decent shape; however, a strangely placed sticker on the top port side turned out to be covering a painful past. Continue reading

WaveRunner repair

Fiberglass Repair on a Yamaha WaveRunner

By Jordan Teddleton

I wanted to purchase a personal watercraft so I’d be able to join my friends at the local lake for some fun in the sun this summer. Like most people on a budget, I searched Craigslist for the best deal. I needed something low maintenance, so a WaveRunner™ felt like a good fit. After a week of looking, I found a 2004 Yamaha GP1300r that appeared to be in decent shape; however, a strangely placed sticker on the top port side turned out to be covering a painful past. Continue reading