Borate Salt Treats Decayed Wood

By Tom Pawlak — GBI Technical Advisor

Sodium borate is used in a number of commonly used household products from laundry detergent to hand soap. It is also used to treat wood against insect and fungal attack. Sodium borate is refined from borax, a natural mineral, which is mined throughout the world. One of the largest deposits is in the Southwestern United States. (Think 20-Mule Team Borax™, Death Valley Days radio and TV shows).