Rebuilding a Rudder

by Barry Duke

Above: The two foam halves of the rebuilt rudder, with the plywood core, are dry fit around the post before bonding.

What started out to be a relatively easy job of replacing the motor mounts and cutlass bearing on my 1983 Nelson/Marek 36 turned into building a completely new rudder. Once I removed the rudder, I had planned on fairing it and applying a WEST SYSTEM® Epoxy with 422 Barrier Coat Additive. barrier coat. However, upon closer inspection, I noticed that the rudder appeared to be bent.

Continue reading