By Tom Pawlak

Construction of fiberglass tubs and showers uses methods and materials similar to those for building fiberglass boats. Gelcoat is applied to a mold and allowed to cure. Then chopped fiberglass and polyester resin are applied over the gelcoat and worked into the surface. To create a stiff and strong fiberglass tub or shower enclosure, the laminator uses a grooved roller to compact the fibers against the gelcoat. The quality and strength of the laminate depends on Continue reading