Tag Archives: skeg

Bonding a Skeg to a Polyethylene Kayak

By Chris Maples

Editor’s note: this article was written in 2000, years before we formulated G/Flex 655 epoxy which has superior performance with plastics. The basic plastic boat bonding methods described here still represent best practices, but for optimal results use these methods with G/flex 655 epoxy on plastics.

The hull shape of a white water kayak is not designed for tracking well in open water. Since I do most of my kayaking on open water and flatter rivers, I decided to mount a skeg on the hull to make it track better. This is pretty simple if you own a wood or fiberglass boat, but can be more challenging on a polyethylene kayak. Continue reading