by William D. Bertelsen
Ticonderoga is a 220 ft. sidewheel steamboat built in 1906. She carried passengers on Lake Champlain until 1953. The Shelburne Museum wanted to replace the decks and cover them in a way that recreated the appearance and texture of the original canvas sheathing. But it was equally important that the authentic looking decks be durable enough to survive the unrelenting foot traffic inevitable for such a magnificent museum centerpiece. Continue reading