Fast Blister Repair with Six10

By Tom Pawlak — GBI Technical Advisor

This fast blister repair method is tailored to fixing individual gel coat blisters prior to bottom painting. The advantage of this method is it can repair blisters on hulls recently pulled from the water or hulls that have been out for some time.

Continue reading

Repairing individual gelcoat blisters

Repairing Individual Gelcoat Blisters

By Tom Pawlak — GBI Technical Advisor

Gelcoat blisters can be a serious problem if left unattended. At some point, your hull may need extensive repair, including gelcoat removal and epoxy barrier coats as described in Gelcoat Blisters: Diagnosis, Repair & Prevention. However, if you have isolated blisters and a manageable number to repair individually, we often recommend that you patch individual blisters and continue to use the boat until you determine the cause and extent of the problem. Continue reading