Gluing Plastic Dimensional Lumber

by Patrick Ropp—GBI Technical Advisor

More people are using recycled plastic/wood composite lumber for decks and other various projects. Although each manufacturer of recycled plastic lumber has his own blend, we found that most are using very similar ingredients: an equal amount of melted recycled plastic mixed with recycled wood chips or sawdust and then extruded in the form of dimensional lumber. Since the wood is encased in plastic, the plastic/wood composite boards are supposed to last longer than traditional decking materials and carry a good warranty. Many of these boards are not intended for use as structural members, but they Continue reading