By Tom Pawlak — GBI Technical Advisor
25 years of use (some might say abuse) had taken its toll on the heavy aluminum rip fence on our Delta Rockwell 12″–14″ Tilting Arbor Saw. Deep saw kerf grooves on the face of the fence had become a hazard because wood occasionally got hung up on it when ripping stock. Over a few months, each time I used the saw I thought about how it could be repaired. While the plan was still developing in my head, more than once I clamped a flat piece of plywood to the rip fence face to temporarily create the smooth surface that I needed.
(more…)