This cedar strip canoe (top) was laminated with WEST SYSTEM® 105 Resin®/207 Special Clear Hardener®. It is the work of Kurt Mangseth of Grand Rapids, Minnesota.
Latest articles by Epoxyworks Community
This cedar strip canoe (top) was laminated with WEST SYSTEM® 105 Resin®/207 Special Clear Hardener®. It is the work of Kurt Mangseth of Grand Rapids, Minnesota.
by Robert Garrison I designed and, with the help of others, built my big, beautiful barn many years ago. While we didn’t use epoxy in the construction, I’ve used WEST SYSTEM® many times to make repairs and modifications. Much of this was needed because the construction crew didn’t follow the design instructions. The fourth floor […]
By Donald Weir Most of the projects featured in Epoxyworks are neat and have a high level of finish. For a creation that will be put in the ocean and beat on with sticks, that seemed too high of a standard. When building the Unlimited Canoe, we instead opted for durability and fast construction, not […]
Wooden rowboat (featured image, above) by Joshua Rouch. Buster Welch’s Boats & Furniture Buster Welch of Clandeboye, Manitoba, Canada has had extensive experience with epoxy. He began with building a cedar strip canoe in 1973 after seeing one of Ted Moores’s (Bear Mountain Boats) on display at the Toronto Boat Show.
By Jeff McAffer It all started when I got a new 360-degree camera for my racecar. Mounted on the dash, it captures a really cool perspective that allows viewers to see forward, watch cars as I pass them, and to see what I’m doing (check it out at youtube.com/user/jeffmcaffer). Unfortunately, the dash produced considerable glare […]