by Jim Derck Why do centerboards and rudders need durable edges? When centerboards and flip-up rudders drag across the bottom, the first fiberglass to abrade away is usually the leading edge at the bottom. This exposes the end grain of the wood, allowing water to be absorbed the length of the centerboard or rudder. The […]