by Jim Derck—GBI Technical Advisor Our 403 Microfibers and 405 Filleting Blend are excellent structural fillers but they’re fibrous and leave a rough surface when used to make fillets. To end up with a surface that is ready for coating or re-bonding without having to remove amine blush or sand smooth, apply a narrow strip […]