By Tom Pawlak — GBI Technical Advisor The appeal of well-maintained, varnished wood trim on boats is hard to deny. It evokes our past and we respect the owner because of all the time and effort it takes to apply and maintain the varnish.
Explore the latest Coating articles
By Tom Pawlak — GBI Technical Advisor The appeal of well-maintained, varnished wood trim on boats is hard to deny. It evokes our past and we respect the owner because of all the time and effort it takes to apply and maintain the varnish.
For Paints and Primers by Joe Parker Above: Surface prep testing using ASTM D3359. This calls for a single-edged razor blade to score a pattern through the coating. Applying a strip of masking tape diagonally across the pattern, then pulling it slowly back over itself will reveal the relative degree of adhesion to the substrate […]
By Tom Pawlak — GBI Technical Advisor Gougeon Brothers, Inc. regularly engages in testing to support those who use our epoxy in architectural applications, both in new construction and repairs. In the past, we have tested the compatibility of house paint primers over WEST SYSTEM® epoxy and found that a variety of primers worked well. Latex […]
By Tom Pawlak — GBI Technical Advisor My porch railing at home was badly in need of painting even though I had painted it the summer before. After just one Michigan winter, the paint had cracked and lifted. I wondered to myself if coating the top rail with WEST SYSTEM® epoxy would improve this poor situation […]
Epoxyworks reader Jim Cronan of St. Ignace, Michigan completed a Phil Bolger designed Martha Jane that he had worked on for five years. He offed a couple of suggestion the helped him with his project.