By Tom Pawlak — GBI Technical Advisor A local sailor stopped by our shop with an old plastic hatch that was slightly warped and badly cracked. He hadn’t been able to find a similar hatch to replace it. He wondered if we had an epoxy that could be used to repair the hatch. I said G/flex […]