by Bruce Niederer — GBI Technical Advisor Above: We mixed and applied a third coat thickened with 406 Colloidal Silica Filler to create the texture for the non-skid finish on the deck. This racing season onboard Triple Threat has been filled with the usual mix of tedium, laughs, and excitement. It’s a good thing when […]