Water beading on a bright finish topcoat.

The Art of Choosing a Topcoat

By Rachael Geerts – GBI Composites Materials Engineer

You’ve just finished your epoxy project and it looks great! But you don’t want the sun’s UV rays to start degrading the epoxy. So, like the smart individual you are, you look into applying a UV stable topcoat over the epoxy so your project will last for years to come. You look at your options, go down a few rabbit holes, and come out much later asking why is it so difficult to select a UV stable topcoat for my epoxy project? Continue reading

Unlimited canoe, completed

Unlimited Canoe

By Donald Weir

Most of the projects featured in Epoxyworks are neat and have a high level of finish. For a creation that will be put in the ocean and beat on with sticks, that seemed too high of a standard. When building the Unlimited Canoe, we instead opted for durability and fast construction, not to mention cheap. Continue reading

Little Free Library

Weatherproofing my Little Free Library

by Grace Ombry

As a novelist and an avid reader, I was captivated by the Little Free Library® (LFL) movement from the moment I learned about it. In the summer of 2019, we set up one of our own and used WEST SYSTEM® Epoxy extensively to ensure that it would remain sturdy while keeping the elements out and the library books dry. Continue reading

Bill Wright, Ian Wright and Tony Riek, Norman R Wright with the hull of Saltash (Left to Right).

High-Tech Composites will Revive Champion Keelboat

Saltash gets a new lease on life

by ATL Composites

The nifty keelboat Saltash—an eight-time winner of Australia’s Brisbane to Gladstone Race—is getting a new lease on life from the craftspeople at Norman R. Wright & Sons using WEST SYSTEM® Epoxy and carbon fiber. Currently upturned in the yard at Norman R. Wright & Sons (and dwarfed by the carbon fiber bulk of the supermaxi Comanche) at the Rivergate complex, the hull and skeletal superstructure of Saltash belie her glorious past and pedigree. Continue reading

Row boat by Joshua Rouch

Readers’ Projects, Issue 52

Wooden rowboat (featured image, above) by Joshua Rouch.

Buster Welch’s Boats & Furniture

Buster Welch of Clandeboye, Manitoba, Canada has had extensive experience with epoxy. He began with building a cedar strip canoe in 1973 after seeing one of Ted Moores’s (Bear Mountain Boats) on display at the Toronto Boat Show.

Strip canoe by Buster Welch

Strip canoe built inspired by Ted Moores and built by Buster Welch.

Continue reading