Tag Archives: Ted Moores

Sealing and Priming

By Ted Moores

This article is Lesson 4 of a series. See bottom of page for links to additional articles in this series.—Ed.

The way a finish ages has everything to do with the way it is anchored to the wood. Sealers and primers are often taken for granted; we simply read the can and follow directions. There are so many reasons for using a sealer and many methods for applying them. Let’s look at what we learned while sealing Sparks, the electric launch I built. Continue reading

Skeg Construction for SPARKS

By Ted Moores

This article is Lesson 3 of a series. See bottom of page for links to additional articles in this series.—Ed.

Designing and building a successful skeg for Sparks (our 30′ hybrid electric launch featured in Epoxyworks 32) took some head scratching. But in the end, it was just another combination of wood and WEST SYSTEM® epoxy. Our skeg needed to be functional and age gracefully, yet be reasonably quick and easy to build and install. This project was an ideal opportunity to explore the limits as well as the advantages of combining wood with epoxy to engineer simple solutions to complex problems. Continue reading

Fiberglassing a Strip-planked Boat

 By Ted Moores

This article is Lesson 2 of a series. See bottom of page for links to additional articles in this series.—Ed.

With our strip-planked hull faired and the outside stem attached, there are many techniques that could turn these strips into a boat.

Strip-planking may have been the first step after the dugout in the evolution of boatbuilding techniques; the way the quality of wood is going, it might be the last to survive. At the La Routa Maya canoe race in Belize, SA., we saw a natural progression from chopping canoes out of logs to strip-plank construction with WEST SYSTEM® Epoxy. Continue reading

SPARKS by Ted Moores

Ted’s Jewel Box

by Michael Barker

Epoxyworks 32

Cover Photo: Ted Moores ties up SPARKS at the blue line at Kilmarnock Lock n the Rideau Canal.

After three years of painstaking work and many interruptions, Ted Moores of Bear Mountain Boats completed the Bear Mountain 30 Hybrid Electric Launch Sparks on June 22, 2010. The boat is unlike any he had built before.

 The Bear Mountain 30 Hybrid Electric Launch is designed for low-speed cruising while using the least amount of fossil fuel possible. It normally runs on batteries charged by solar panels and shore power. When necessary, a diesel generator powers its electric motor and charges its batteries. Continue reading

Strip Planking SPARKS

By Ted Moores

This article is Lesson 1 of a series. See bottom of page for links to additional articles in this series.—Ed.

Sparks is a science project. A professional builder working for a client has the responsibility of delivering the boat on time and budget with no surprises so we generally stick to what worked last time. But as a science project, questioning the way things are usually done, pushing the limits of the materials and then taking the responsibility becomes the objective. Because failure is anticipated with any experiment, testing is an important part of the project and has been a whole lot of fun with few surprises, mostly pleasant.

Continue reading

Testing for Damage Tolerance

By Jeff Wright — Vice President of Technical Services

Ted Moores and his company, Bear Mountain Boats, build wood epoxy strip plank canoes, manufacture kits and publish books on building strip plank canoes and kayaks. This method of construction provides a very light yet stiff structure and also enables the hull shape to have compound curves. Moores has 30 years of experience and his designs have logged many safe miles. He understands the forces boats are subjected to when paddled on the water and during transportation. Continue reading

Fiberglassing a Woodstrip Hull

By Ted Moores

The WEST SYSTEM User Manual describes the basics of fiberglass cloth application and coating for clear finishing over wood. This article is the ultimate guide to applying fiberglass over a woodstrip hull to achieve a perfect finish. Ted Moores is a master of the perfect finish, author of CanoeCraft and KayakCraft and co-owner of Bear Mountain Boats. Continue reading

Bear Mountain Boats

Bear Mountain Boat Shop, owned by partners Ted Moores and Joan Barrett, is well known for pioneering effective methods of woodstrip epoxy small boat construction and for sharing that expertise with amateur builders around the world. CanoeCraft and KayakCraft, written by Ted Moores, have encouraged thousands to build light weight wooden craft with professional results while using the most advanced materials available. Ted’s fascination with canoes and heritage craft began in 1972. Since that time, the company has built and restored numerous boats from mahogany runabouts to the fastest sprint racing canoes on the market. Continue reading

Bear Mountain boats

Bear Mountain Boat Shop

Your Canoe Building Connection

People from all over the world have read Canoecraft by Ted Moores & Marilyn Mohr. This illustrated guide to building a strip canoe has helped many first time builders create elegant canoes. Bear Mountain Boat Shop is the company behind the book, a family business that has much to offer the strip canoe builder. Continue reading