The Marita is a modern, live edge coffee table made out of a solid 2.25″ thick slab of Canadian Black Walnut salvaged from Essex County, Ontario. The void in the center of this curly black walnut slab was filled with broken safety glass and WEST SYSTEM Epoxy. The table is lit from below with a […]