Above: Pouring an air-free transducer base for installing a depth sounder. Draining neat (unthickened) epoxy through a hole in the bottom of the mixing cup will leave the air bubbles behind on the surface. A putty dam on the hull ensures the correct size and shape for the depth sounder base. Jim Costello of Dallas, […]