By Don Gutzmer – GBI Technical Advisor The advantage of repairing a keel with G/flex Epoxy is that it is a toughened system that has a tensile elongation of more than 30 percent, which would prevent cracks from reappearing in the fairing compound. A local boat owner called our technical line and asked about repairing […]