By Dan Anderson Above: Align stitch-and-glue panels with a dowel rod. The wire connecting the panel edges passes over the dowel section on the inside of the joint, clamping the panel edges to the dowel. Here’s a tip for when you need to align stitch-and-glue panels that we heard about too late to use on […]