by Tom Pawlak — GBI Technical Advisor Above: Tom’s transom saving tip is to epoxy conveyor belt material into place, protecting the transom wood from getting crushed by the motor mount screws. Ten years ago, I replaced the plywood transom in my 16′ aluminum fishing boat. It had gone bad due to the motor mount […]